i want to remove the chrome strips from the side of a 65 beetle and fill in the holes , what would be best some sort of bog or weld them . i think
the welder would distort the metal . if i use bog do i just poke it into the hole`s
|
|
68AutoBug
A.k.a.: Lee Noonan
Aircooled Master
Beetle Restorer - Experience over 138% - YIKES --
Posts: 11654
Threads: 449
Registered: August 31st, 2002
Member Is Offline
Location: SCONE in UPPER HUNTER VALLEY NSW
Theme: UltimaBB Pro Yellow
Mood: Really Mentally Ill - all of the time -
|
posted on February 9th, 2004 at 11:04 AM |
|
|
I had mine brazed up, with bronze. However You do it, when welding or brazing, You have to be careful NOT to heat the metal too much, as it will
distort.
I can't really see any problem with using Bog, just make sure the interior of the holes are nice and clean for the bog to bind to. I myself
wouldn't try to weld them... You would have to know what You are doing.
Best of Luck.. Lee
- [size=4]Helping keep Air Cooled VWs on the road - location: SCONE in the Upper Hunter Valley - Northern NSW 320 kms NNW of SYDNEY--- [/size]
|
|
68AutoBug
A.k.a.: Lee Noonan
Aircooled Master
Beetle Restorer - Experience over 138% - YIKES --
Posts: 11654
Threads: 449
Registered: August 31st, 2002
Member Is Offline
Location: SCONE in UPPER HUNTER VALLEY NSW
Theme: UltimaBB Pro Yellow
Mood: Really Mentally Ill - all of the time -
|
posted on February 9th, 2004 at 11:10 AM |
|
|
I would fill the holes up from the inside,
so make sure its clean around the holes & leave some bog inside the door to give them some strength. If You just filled the holes from the
outside, there wouldn't be much holding the bog in the hole... and it may fall out...
Lee
- [size=4]Helping keep Air Cooled VWs on the road - location: SCONE in the Upper Hunter Valley - Northern NSW 320 kms NNW of SYDNEY--- [/size]
|
|
BJ
Seriously Crusin Dubber
Posts: 177
Threads: 48
Registered: November 19th, 2003
Member Is Offline
Location: Toowoomba
Theme: UltimaBB Pro Blue ( Default )
Mood: COOL
|
posted on February 9th, 2004 at 11:25 AM |
|
|
I just finished doing mine on a 1960 beetle and found the best way is to tape up the inside and push back to form a bulge then work the bog around to
spread on the inside then smooth on the outside. You may not like this as some of the holes and fill show on the inside.
|
|
helbus
A.k.a.: Pete S
Super Administrator
Mad fabricator, paint and body
Posts: 7386
Threads: 312
Registered: September 1st, 2002
Member Is Offline
Location: In the garage chopping cars into bits
Theme: UltimaBB Pro Blue
Mood: In the thinking chair
|
posted on February 9th, 2004 at 05:10 PM |
|
|
I wouldnt recommend filler if you want to last.
Welding does distort the metal slightly.
The best way to do it is solder.
The hole needs to be cleaned so the edges are bare metal. A small round file will do this nicely so you dont take any metal out, only clean the
edges.
If you use an old style soldering iron. The ones that are a big copper block with the pyramid shaped end.
The iron should be held in the hole and solder fed in. Then draw the iron out while twisting it. The twisting action keeps the solder in the hole like
a soap bubble over a hole.
This will cool and harden. It can then be filed or sanded level. Some of the holes will have a tiny dip in them, but they can be filled with
filler.
This procedure is pretty much permenant, unless you heat it up.
Best of all it doesnt distort the metal.
|
|
wadd
Seriously Crusin Dubber
Posts: 179
Threads: 41
Registered: April 6th, 2003
Member Is Offline
Location: Mt Isa Qld
Theme: UltimaBB Pro Blue ( Default )
Mood: sunny
|
posted on February 10th, 2004 at 08:14 PM |
|
|
thanks for the reply guys i might try the solder as some panels are double and you carn.t get to the inside of them
|
|
Buggyboy
Officially Full-On Dubber
Posts: 255
Threads: 46
Registered: October 9th, 2003
Member Is Offline
Location: Brisbane
Theme: UltimaBB Pro Blue ( Default )
|
posted on February 22nd, 2004 at 02:53 PM |
|
|
Am just a novice with these panel things, but I know enough not to just use bog and chicken wire.
Anyway my soldering experience has only been limitted to electrical toys (Just to clarrify childrens toys, not adult toys) and I am assuming that it
is the same theory but with different materials and soldering iron. Could you recommend a sort and product.
I am restoring a country buggy which has more holes than metal and thought that I could fill a lot of the holes with the mig (being mindful of
destortions) and will do so for the larger jobs- I am getting a lot of the metal folded and hope to replace rather than repair, but was more
interested in those little 2-3ml holes that appear from time to time.
thanks
Peter
|
|