Aluminum Paint workshop
I have an engine lid badge - 1300 badge - made out of aluminum.
Its an old replacement - and it looks dull and white patchy.
I read up about how it has be acid dipped, etch primed and a fair bit of prep work to paint it. It all seems a fair amount of work for a small bit of
metal for me.
Is there a good shop that will do that for me instead?
______________________
Owner of a 1964 VW Beetle, 1641cc engine, etc..
vw54
Super Administrator
Always Waiting 4 Friday
Posts: 16723
Threads: 378
Registered: August 26th, 2002
Member Is Offline
Location: Sunny Sydney
Theme: UltimaBB Pro Blue ( Default )
Mood: Oval resto ongoing
posted on December 31st, 2015 at 03:37 PM
they are usually die cast metal