Does anyone out there know how to paint magnesium componets in such a way that it doesn't allow the magnesium to breath so much that it creates bubbles under the paint???

vw54 Administrator Always Waiting 4 Friday

16,723 posts · joined Aug 2002 ·

#631057
yes i believe that you have to chemically treat the surface B4 you apply the paint

at Qantas we used to apply some chemicals to new machined surfaces which bonded into the surface of the magnesium i think it was called Iridite or something like that talk to your local electroplating shop itsa similar process to anodising

It would also help if you wash the parts down with Kero then degreased with some acetone then even baked the item at 100 D C fora while to bake out all the surface abnormalities
I read it on FACEBOOK so it must be true


http://forums.aussieveedubbers.com/viewtopic.php?tid=91278&page=1#pid848630


http://forums.aussieveedubbers.com/viewtopic.php?tid=63561&page=1#pid624099


http://forums.aussieveedubbers.com/viewtopic.php?tid=4832&page=1#pid452603


http://forums.aussieveedubbers.com/viewtopic.php?tid=60650&page=1#pid574409

063bug

0 posts · joined Feb 2005 ·

#631065
Thanks for that vw54. I have spoken to a mob that does ceramic coating but they say they can't do it. Is ceramic coating the same as anodizing?