Skip to content
Aussieveedubbers

Anyone use standox??

0 likes
Share Share on Facebook Share on X Share on Reddit

Zimblewinder Seriously Crusin Dubber

109 posts · joined Feb 2004 ·

#394140
I heard they were one of the companies that did the original VW codes and they still do Sealing wax red. Havent used it before myself and was hoping someone could lead me through the products from metal to topcoat. Any quirks, comments about this stuff? Its that or Glasurit but Id prefer to lose an arm instead of both my arms and legs to the paint job ($$$$).

Cheers
Dalenn[ Edited on 5-8-2005 by Zimblewinder ]

killakornkobb where's that clutch?

1,663 posts · joined Mar 2004 ·

#394192
sorry havnt used standox, but glasurit is the shiznit🙂
Tagedeezee Heezy

decked dubby Custom Title Time!

1,046 posts · joined Aug 2002 ·

#394282
My oppinion from experience is PPG is the best, House of colour the worst. Had problems with clear with Glasurit, changing colour. Standox is ok. You genrally get what you pay for.
.

DubCrazy Custom Title Time!

1,295 posts · joined Jul 2003 ·

#394336
All of the main brands will be able to do products that are of a good standard, which one you use comes down to what your prefer.. i personal think ppg is at the lower end of the spectrum with glasurit being towards the top.. i have used most paint systems over the years and if your willing to spend glasurit is one of the best. cheaper but almost as good are spies hecker,sikkins ( i currenty work in a shop with spies and i cant fault it great stuff) even lesonal is worth a look..

As for the comment on "house of kolor" there range is only aimed at full custom paint work and u will be hard pushed to get better candy etc... not a fan of there clears but thats not saying they aint good,bloody expensive stuff tho... have a look in the fixed topics on the main paint/body page and there is detailed step by step guides on how to.....


steff........................
Life with out a v-dub is no life at all!!!!!

decked dubby Custom Title Time!

1,046 posts · joined Aug 2002 ·

#394438
House of colour is the worst paint to use......... Nice colour range, just shit paint. Any house of colour paint colour can be duplicated with other brands.

All PPG :

nn[ Edited on 6-8-2005 by decked dubby ]
.

DubCrazy Custom Title Time!

1,295 posts · joined Jul 2003 ·

#394441
as i said decked, its a matter of opinion.. i have been useing house of kolor for many years and have always had great results.. i dont know the circumstances you have used them in so cant comment but your the first i have ever heard that thinks that way..... when it comes down to it its all personal choice... like whats better iwata or sata, one painter will say one thing another will say different... as long as each is happy with what they use and the end result is the same who cares?


steff............
Life with out a v-dub is no life at all!!!!!

decked dubby Custom Title Time!

1,046 posts · joined Aug 2002 ·

#394447
Yep, personal opinions...........
.

Che Castro ankle straps

1,945 posts · joined Aug 2002 ·

#394599
Ive used standox 2k and PPG Cobra. Both seemed pretty high quality to me - I think it'd be fair to say that the quality of the finish would probably be more attributed to the prep work and how its applied rather than the paint system you use.

I have looked myself for a lot of original VW colours in the PPG range, and most of them are in Acrylic or not in Cobra anyway. So if you decide on a certain paint system and/or you want to do 2k, just get it colour matched.
Jon

5PL1TDCS10N Insano Dub Head

845 posts · joined Jan 2003 ·

#395141
Hi Z,

Get the best etch primer you can(epoxy) as a base. This will protect the precious metal thats under the paint. As for the color what you will be using are base colors so you should find that most higher market paints are equal: DeBeer, PPG, Standox, Glasurit. Leave HOK for kandy's and pearls....
Glasurit will guarantee your paint for life if used as a complete system and by a qualified painter. That in itself speaks volumes on the quality imo

Zimblewinder Seriously Crusin Dubber

109 posts · joined Feb 2004 ·

#396093
Thanks All, Im pretty much stuck with Glasurit or Standox cos theyre the only ones who produced the OG formula sealing wax red. Any one can match this paint at shop but it has a very poor fade life, ie most other makes dont look anything like it after a year or two's life. Im not to worried about either paint cos their reputuations are A1, I was only really concerned with how they shoot for the first time user. Ive been ok with PPG and Sikkens before but never either of these two. No one really has anything bad to say about the undercoats and basecoats so its pretty much down to how much I want to spend.

Thanks alot
Dale

helbus Administrator Mad fabricator, paint and body

7,386 posts · joined Sep 2002 ·

#396180
All paint companies have reformulated their paints that contained high lead content. This was a requirement starting in the mid 80's and pretty much stopping all lead in the paint by the end of the 90's

Red, Yellow an White tinters used to contain as much as 30% lead oxide. It is the lead oxide that gives those coulours their 'balls' that is coverage and resistance to fading. This is why so many mid 80's to mid 90's red cars faded within a year or two.. The paint companies could not come up with alternatives quicker than the lead content was dropping.

Not such a problem now with the major companies. Also PPG makes pigments for a lot of other paint companies. 2/3 of all new OEM paint finishes contain PPG pigments.
EJ22 into Bay Microbus - Finished project build thread- click on this spot here for info

Che Castro ankle straps

1,945 posts · joined Aug 2002 ·

#396330
wow didn't know that about PPG pigments. learn something every day.
Jon