satori Wolfsburg Wizard 497 posts · joined May 2008 · 15 Jul 2008, 9:36 pm #657933 Hey everyone. Just wondering what to do to surface rust that has formed on bare metal before spraying with etch primer??? [URL=http://s1226
helbus Administrator Mad fabricator, paint and body 7,386 posts · joined Sep 2002 · 15 Jul 2008, 10:01 pm #657946 A phosphorous acid metal surface treatment. Some brand names are De-Ox-It, Deoxidine, Deran-A etc. Follow the instructions as supplied by the manufacturer. EJ22 into Bay Microbus - Finished project build thread- click on this spot here for info
satori Wolfsburg Wizard 497 posts · joined May 2008 · 16 Jul 2008, 12:00 pm #658049 Great, thanks. [URL=http://s1226