Does anyone know of somwhere near Brisbane that can do this?
Alt who does good panel work. lots of small holes etc in bottom of front and rear gaurds. (usual spots)
Also some larger ones which would require a bit more work.
Was going to have a crack at this but is getting a it daughting and time is hard to find at the mo.
Really want to try and stay away from the putty quick fix if possible.
Also the bottom of one of the doors has a large hole in the bottom of the door, only visable from bottom,is on the inside and not visable from out side.
Is this repairable or a waste of time. would like to try and keep all as i got.
Left hard drive at home with pic's will post some later.

HappyDaze Superannuated

2,887 posts · joined Jun 2009 ·

#964112
Sound like a bit more than lead-wiping required, although it's hard to tell without seeing the damage.

I did quite a bit of lead-wiping in the '50s - early '60s, but lead is not good over rust. Pity you are so far away, or I could give some lead-wiping lessons.
I'd rather wear a Beetle out by racing it than by polishing it!

vw54 Administrator Always Waiting 4 Friday

16,723 posts · joined Aug 2002 ·

#964128
yep Lead wiping is really only for the seams in the old days before BOG was invented

hardtop do as you must have a ultra clean surface and require a good flux also

nothing wrong with the plastic body filler these days much easier to use and safer ( also you must have a good clean surface to bond to )
I read it on FACEBOOK so it must be true


http://forums.aussieveedubbers.com/viewtopic.php?tid=91278&page=1#pid848630


http://forums.aussieveedubbers.com/viewtopic.php?tid=63561&page=1#pid624099


http://forums.aussieveedubbers.com/viewtopic.php?tid=4832&page=1#pid452603


http://forums.aussieveedubbers.com/viewtopic.php?tid=60650&page=1#pid574409

Matty v Commited Dubber

55 posts · joined Jul 2010 ·

#964164
Thanks for the replies, i have been cutting and welding in patches, (fun weliding such thin material) for the larger holes etc, the areas i was thinking about leading are areas where there is pitting not all the way through the panel, sort of on the curve/bends. appears to have cleaned up quite well but may just have to look at the plastic stuff.
Will post some piccies when i get a chance for your opinion.
Shame im not closer happdayz for sure, i would still love to check out this old practice and try and keep the skill alive.
Thanks for the advice, trying to sort this has slowed my restro but in no rush.

vlad01 Compulsive Aussie Vee Dubber

4,270 posts · joined Jun 2010 ·

#964250
Matty v wrote:Thanks for the replies, i have been cutting and welding in patches, (fun weliding such thin material) for the larger holes etc, the areas i was thinking about leading are areas where there is pitting not all the way through the panel, sort of on the curve/bends. appears to have cleaned up quite well but may just have to look at the plastic stuff.
Will post some piccies when i get a chance for your opinion.
Shame im not closer happdayz for sure, i would still love to check out this old practice and try and keep the skill alive.
Thanks for the advice, trying to sort this has slowed my restro but in no rush.
you will have real difficultly lead filling pitted areas, been there done that. even sand blasted clean the flux and lead was hard to flow.


As hellbus said, need to be perfect and super clean metal for it to be effective.

Its good on joins and overlaps, seams and minor dents that can't re otherwise accessed via panel beating tools.

beats the hell out of bog imho, wont touch that shit!